Abstract
Pipe specimens made of commercial grade galvanized steel and zinc have been tested in comparison to pipe specimens having modified zinc coatings. The specimens were corroded in 11 test lines with warm water at approx. 60 degree C and cold water with continuous and intermittent flow. The investigation included visual assessment, determination of mass loss, and electrochemical measurements.