Equipments Details
Description
The Kappa SS-CF 100 is an electromechanical creep testing machine by ZwickRoell, developed for demanding tests under alternating loads. With a maximum test force of 100 kN, it is suitable for force- and strain-controlled creep fatigue tests. Thanks to its backlash-free central spindle drive, it offers maximum flexibility and precision for a wide range of applications.
Capabilities and Tests That Can Be Performed:
Tensile tests at elevated temperatures (up to 1,100 °C)
Tensile tests at room temperature (limited capacity)
Testing of creep and relaxation behavior at elevated temperatures (up to 1,100 °C)
Low-cycle fatigue testing (LCF) at elevated temperatures (up to 1,000 °C)
Creep-fatigue testing at elevated temperatures (up to 1,000 °C)
Tensile tests on small specimens at elevated temperatures (up to 1,100 °C)
Capabilities and Tests That Can Be Performed:
Tensile tests at elevated temperatures (up to 1,100 °C)
Tensile tests at room temperature (limited capacity)
Testing of creep and relaxation behavior at elevated temperatures (up to 1,100 °C)
Low-cycle fatigue testing (LCF) at elevated temperatures (up to 1,000 °C)
Creep-fatigue testing at elevated temperatures (up to 1,000 °C)
Tensile tests on small specimens at elevated temperatures (up to 1,100 °C)
Fingerprint
Explore the research areas in which this equipment has been used. These labels are generated based on the related outputs. Together they form a unique fingerprint.