Abstract
The use of a scaffold processing method on an injection molding machine was described. The granulates were injection molded into an aluminum mold with a cyclic time of 45 seconds. Thermal degradation were monitored by a Annotated Total Reflexion Fourier Transform-Infrared and Gel Permeation Chromatograph. The polyurethane scaffolds have a mean pore size of 100 μm and porosity of 60%.