Concentration of surface hydroxyl groups on MCM-41

A. Jentys, K. Kleestorfer, H. Vinek

Publikation: Beitrag in FachzeitschriftArtikelBegutachtung

150 Zitate (Scopus)

Abstract

The type and concentration of hydroxyl groups present on MCM-41 were investigated by infrared spectroscopy as a function of the Si/Al ratio and the pore size. The purely siliceous samples contained the highest concentrations of weakly acidic silanol groups. On aluminum-containing MCM-41 samples additionally Brønsted and strong Lewis acid sites were observed. Their concentration increased with increasing aluminum content, while that of the weakly acidic silanol groups decreased. For MCM-41 samples prepared with C12TMABr, higher concentrations of weakly acidic hydroxyl groups and strong Lewis acid sites, and lower concentrations of Brønsted acid sites, were observed compared with MCM-41 prepared with C16TMABr. Comparison of the spectroscopic data with the results of a structure simulation revealed that the internal surface of MCM-41 is only partially covered with hydroxyl groups.

OriginalspracheEnglisch
Seiten (von - bis)321-328
Seitenumfang8
FachzeitschriftMicroporous and Mesoporous Materials
Jahrgang27
Ausgabenummer2-3
DOIs
PublikationsstatusVeröffentlicht - Feb. 1999
Extern publiziertJa

Fingerprint

Untersuchen Sie die Forschungsthemen von „Concentration of surface hydroxyl groups on MCM-41“. Zusammen bilden sie einen einzigartigen Fingerprint.

Dieses zitieren