Zur Hauptnavigation wechseln Zur Suche wechseln Zum Hauptinhalt wechseln

Capacity Recovery Effect in Commercial LiFePO4 / Graphite Cells

  • Technische Universität München

Publikation: Beitrag in FachzeitschriftArtikelBegutachtung

46 Zitate (Scopus)

Abstract

We report a significant capacity recovery effect of more than 10% after continuous shallow cycling of commercial LiFePO4/Graphite cells. In a previous study on a LiFePO4/Graphite cell, we observed that capacity losses were more severe with shallow cycles than with full cycles. Herein, the effects of shallow cycling on aging are investigated in detail using three different LiFePO4/Graphite cell models, two 26650-type and one 18650-type. It is shown that a large portion of the capacity losses that occur with shallow cycling can be recovered by holding the cells at 0% or 100% state of charge. Differential voltage analysis and post-mortem experiments suggest that these capacity losses are caused by strongly non-uniform lithium distributions in the electrodes. Hypothetical mechanisms are presented and discussed that could lead to such non-uniform distributions of lithium.

OriginalspracheEnglisch
Aufsatznummer040526
FachzeitschriftJournal of the Electrochemical Society
Jahrgang167
Ausgabenummer4
DOIs
PublikationsstatusVeröffentlicht - März 2020

UN SDGs

Dieser Output leistet einen Beitrag zu folgendem(n) Ziel(en) für nachhaltige Entwicklung

  1. SDG 7 – Erschwingliche und saubere Energie
    SDG 7 – Erschwingliche und saubere Energie

Fingerprint

Untersuchen Sie die Forschungsthemen von „Capacity Recovery Effect in Commercial LiFePO4 / Graphite Cells“. Zusammen bilden sie einen einzigartigen Fingerprint.

Dieses zitieren